    Re: Acid copper not bond on flash copper help

    The Flash copper is strongly alkaline. Make sure you thouroughly scrub and rinse the part before proceding to any other plating and always remember the steps of de-grease and activate if you have handled the parts in any way.

    cheers

    Leave a comment:


  • tcam2
    replied
    Re: Acid copper not bond on flash copper help

    You might want to check the acid copper temperature. I had the same problem until I upped my solution temperature from 100 degrees to around 120.

    Leave a comment:


  • jimcarry
    replied
    Re: Acid copper not bond on flash copper help

    Smokeycity is right what substrate are you working with.
    Then in between flash and acid copper steps are you polishing the piece or
    just rinsing and moving to the acid copper. What grit paper are you using and
    what kind of pressure this is a very light sanding process.
    When asking a question or giving an answer we should all try to be as specific as possible
    Last edited by jimcarry; 11-15-2005, 07:50 AM.

    Leave a comment:


  • smokeycity
    replied
    Re: Acid copper not bond on flash copper help

    what are you plating steel ,pot metal,brass we need info

    Leave a comment:


  • mgcobra
    started a topic Acid copper not bond on flash copper help

    Acid copper not bond on flash copper help

    When i sand the part the acid copper peels off .