    Plating plastic is NOT trivial. It requires lots of practice and patience.

    You'll need to copper paint, copper plate, then Electroless Krome.

    Also see our Silvachrome Kit at http://www.caswellplating.com/silvachrome.html, which is an easier process.

    Leave a comment:


  • strom
    started a topic Plating Plastic

    Plating Plastic

    I have some plastic interior pieces in my car that i would like to rechrome. I was wondering what would be the most inexpesive kit i could use to get a decent looking finsh with. I saw the copper powder stuff and the ELECTROLESS Krome kit and was wondering if this would work on plastic.