    Hi all, I have made a real bonehead move. I mixed my Copy Cad bath with my Zincate! I thought it was my Cad top off container.

    This morning there were crystals attached to my anode and tank
    sides. Am I thouroughly screwed? Can I recover my ZN solution? I am in
    the middle of plating some valve covers on my Porsche 914.

    Thanks MG911Guy.

  • #2
    Re: Bone Head Move with my Copy Cad Bath

    You're not the first person to do this, so don't feel bad. The similarities in the name can be confusing...

    Sorry to say, you won't be able to recover the bath.

    Please give us a call (late Tuesday as our phone's are currently down) and ask for Lance and I'll see what I can do for you.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com

    Comment


    • #3
      Re: Bone Head Move with my Copy Cad Bath

      Thanks for the reply. I have placed an order to replace my copy cad makeup. Oh and I have a Big A** Red Sharpie just waiting to be used.

      Thanks again... Mark...