Caswell and community,
Please help. I have been plating with the black krome very successfully until about 2-3 days ago. I checked my ph level and it seems to be to low. It currently is in the 8-9 ph range. How do I raise it back up into the 11.5 ph range?
Thank you,
Sarah
Please help. I have been plating with the black krome very successfully until about 2-3 days ago. I checked my ph level and it seems to be to low. It currently is in the 8-9 ph range. How do I raise it back up into the 11.5 ph range?
Thank you,
Sarah
Comment