    replied
    Re: copper or pit stop for repairs?

    Can you give me an idea of the size of the pitstop tubes. 1.3 cu. in. means very little to me. Can you compare that to something else?

    Thanks,
    Rick

    Leave a comment:


  • jimcarry
    replied
    Re: copper or pit stop for repairs?

    Rick.
    With the plug and plate you wont be able to get the kind of coverage you need to be able to fill in pits. For this you would need to plate in a bath using flash copper then acid copper .
    Your best bet would be sanding or pit stop

    Leave a comment:


  • rickr_ohio
    started a topic copper or pit stop for repairs?

    copper or pit stop for repairs?

    Which would be better. These are for custom fencing swords, so they need to take some abuse. I have the plug and plate kits. Would I be better of copper plating, sanding, or using pitstop?