    Thanks alot guys
    all has been very helpful

    Leave a comment:


  • mcaswell
    replied
    Re: gold plug n plate over nickel plate

    The gold won't touch nail polish. You can use nail polish as a masking agent without a problem.

    Leave a comment:


  • fxstcguy98
    replied
    Re: gold plug n plate over nickel plate

    As long as the gold solution doesn't disolve the nail polish. Try it and find out.

    Leave a comment:


  • punisher001
    replied
    Re: gold plug n plate over nickel plate

    thanks for that advise.
    i have been told that nail polish will also work and can be removed with naul polish remover ,, is there any truth to this statement
    thanks

    Leave a comment:


  • fxstcguy98
    replied
    Re: gold plug n plate over nickel plate

    you could use laquer paint and use paint remover to take it off when you are finished. Or you get get electroplating tape and mask it.

    Leave a comment:


  • punisher001
    started a topic gold plug n plate over nickel plate

    gold plug n plate over nickel plate

    i have some small parts that have been engraved in solid brass then have been nickel plated at my nearest plating company. i have just purchased the gold plug n plate kit as i want to dual plate the parts.
    The raised areas of the plates will be gold plated and the un-raised areas will stay as Nickel. My question is what is the best way of protecting the nickel so as i don't gold plate the areas i don't want gold plated.