    Re: Gold plug n plate over Nickel

    I'm not trying to hijack the thread or anything, but can I Gold plate over silver plate also? Anything additional I need to do to prep? Thanks,

    Bariman
    Last edited by Bariman; 01-22-2006, 01:55 PM.

    Leave a comment:


  • jimcarry
    replied
    Re: Gold plug n plate over Nickel

    Simple Green , Dawn dishwashing soap and hot water

    Leave a comment:


  • mcaswell
    replied
    Re: Gold plug n plate over Nickel

    Soft Scrub or Dawn and hot water.

    Leave a comment:


  • punisher001
    replied
    Re: Gold plug n plate over Nickel

    Thanks guys
    What is the best thing to use to degrease the part?

    Leave a comment:


  • jimcarry
    replied
    Re: Gold plug n plate over Nickel

    I also do alot of brush plating feel free to call with any questions
    479-639-2575

    Leave a comment:


  • fly
    replied
    Re: Gold plug n plate over Nickel

    If you have anymore questions let me know I did a lot of brush plating and I even have to gold plate a emblum this weekend for Maaco on a nisson.

    Leave a comment:


  • mcaswell
    replied
    Re: Gold plug n plate over Nickel

    Polish the nickel, degrease it, then plate it.

    Leave a comment:


  • punisher001
    started a topic Gold plug n plate over Nickel

    Gold plug n plate over Nickel

    Can anyone tell me how to prepare the Nickel (which has covered over solid brass) for the gold plug n plate