  • Gold plug n plate over Nickel

    Can anyone tell me how to prepare the Nickel (which has covered over solid brass) for the gold plug n plate
    regards

  • #2
    Re: Gold plug n plate over Nickel

    Polish the nickel, degrease it, then plate it.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com

    Comment


    • #3
      Re: Gold plug n plate over Nickel

      If you have anymore questions let me know I did a lot of brush plating and I even have to gold plate a emblum this weekend for Maaco on a nisson.
      www.chrome-plater.blogspot.com

      Comment


      • #4
        Re: Gold plug n plate over Nickel

        I also do alot of brush plating feel free to call with any questions
        479-639-2575
        Jim Eaton

        Comment


        • #5
          Re: Gold plug n plate over Nickel

          Thanks guys
          What is the best thing to use to degrease the part?

          Comment


          • #6
            Re: Gold plug n plate over Nickel

            Soft Scrub or Dawn and hot water.
            --
            Mike Caswell
            Caswell Inc
            http://www.caswellplating.com
            Need Support? Visit our online support section at http://support.caswellplating.com

            Comment


            • #7
              Re: Gold plug n plate over Nickel

              Simple Green , Dawn dishwashing soap and hot water
              Jim Eaton

              Comment


              • #8
                Re: Gold plug n plate over Nickel

                I'm not trying to hijack the thread or anything, but can I Gold plate over silver plate also? Anything additional I need to do to prep? Thanks,

                Bariman
                Last edited by Bariman; 01-22-2006, 01:55 PM.