For the Copy Chrome could I use a 12 volt 2amp charger to power or does it have to be a 6 volt?
Announcement
Collapse
No announcement yet.
Rockie Power Supply?
Collapse
X
-
Yes, you can use a 12V supply. If you read the power supply section of the manual (Page 20), it explains how to set this up correctly.
Also, look on the new web page. There are some tutorials and videos
See the Flash video on 'Controlling the Power Using Light bulbs'.--
Mike Caswell