    Hi.
    This is probably a question for caswell, would it be possible to rate your kits based on the finish corrosion resistance, durability, hardness, have a finish deteriration described, sample colors, etc? Sort of like a comparison table. I have troble deciding what kit do I need given the requirements. Making an obvious mistake would be costly and unnecessary. If I could for example see that Triple Chrome kit produces a 10 rated corrosion resistant finish and Electroless Nikel is 6, it would help in my decision making. But then again I am new to this and maybe talking nonsence, all I know is that there are others like me who do not know much at first. Thanks.
    Andrew.

  • #2
    Perhaps it would help if you described your project to us?

    Chrome will resist tarnish slightly better than nickel.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com

    Comment

    Working...
    X