Re: Titanium Wire For Anodes
Hi,
I use titanium as both the anode and cathode and have no problems at all, my entire anodizing rack is titanium. It will need to be cleaned occasionally.
Announcement
Collapse
No announcement yet.
Titanium Wire For Anodes
Collapse
X
-
Re: Titanium Wire For Anodes
Hello,
It?s ok and will not affect the plating. The plating industry uses titanium baskets for some plating tanks but normally for zinc its steel depending if it?s an acid or alkaline zinc bath.
Nol4154
Titanium Wire For Anodes
I was wondering if any of you guys would know if I can use Titanium wire to hang my anodes in my plating bath for my zink plating system. The reason is I would like to try to submerge the complete anode. Would this effect the finish at all? it would also let me try different position of the anodes as my tank is odd shaped. Thanks
Leave a comment:
-
Re: Titanium Wire For Anodes
I use titanium fasteners and hooks for holding my anodes. the only thing that builds up on them over time is "white rust" which I clean off in before each use.
Cheers
Mark
Leave a comment:
-
Re: Titanium Wire For Anodes
Just wondering if the zinc would eventually build up on the titanium?
Leave a comment:
-
Titanium Wire For Anodes
I was wondering if any of you guys would know if I can use Titanium wire to hang my anodes in my plating bath for my zink plating system. The reason is I would like to try to submerge the complete anode. Would this effect the finish at all? it would also let me try different position of the anodes as my tank is odd shaped. ThanksTags: None
Leave a comment: