I was wondering if any of you guys would know if I can use Titanium wire to hang my anodes in my plating bath for my zink plating system. The reason is I would like to try to submerge the complete anode. Would this effect the finish at all? it would also let me try different position of the anodes as my tank is odd shaped. Thanks
Announcement
Collapse
No announcement yet.
Titanium Wire For Anodes
Collapse
X
-
Re: Titanium Wire For Anodes
Hello,
It?s ok and will not affect the plating. The plating industry uses titanium baskets for some plating tanks but normally for zinc its steel depending if it?s an acid or alkaline zinc bath.
Nol4154
Titanium Wire For Anodes
I was wondering if any of you guys would know if I can use Titanium wire to hang my anodes in my plating bath for my zink plating system. The reason is I would like to try to submerge the complete anode. Would this effect the finish at all? it would also let me try different position of the anodes as my tank is odd shaped. Thanks
Comment