Has anyone had aluminum parts come back that were pealing, I had a 2000 Harley that I had done last april and it showed up at my shop looking the same way it did back then, and I did everything the same as I always do, zinc-nitric acid-zinc, copper and so on, so is it the parts that harley used that are realy the problem. I had heard that harley used some bad parts during those yrs, so can it realy be the material or what, the customer is willing to let me make the call, so do I try it again or what....