Re: calculating credits
see page 149 of the manual. As long as your figure (6000) does not exceed the 70% minimum efficiency level you are okay. You can add during the operation to keep the level from falling past 30% use or depletion.
Announcement
Collapse
No announcement yet.
calculating credits
Collapse
X
-
calculating credits
I have just bought a Electroless nickel plate kit but i can't work out how to calculate the credits.
i have several brass plates that are about 200 sq" surface area and want to immerse them for 30 minutes
i have worked it out that it will be 6000 credits but from there i don't know what to do next