    I have just bought a Electroless nickel plate kit but i can't work out how to calculate the credits.
    i have several brass plates that are about 200 sq" surface area and want to immerse them for 30 minutes
    i have worked it out that it will be 6000 credits but from there i don't know what to do next
    any help will be great

  • #2
    Re: calculating credits

    see page 149 of the manual. As long as your figure (6000) does not exceed the 70% minimum efficiency level you are okay. You can add during the operation to keep the level from falling past 30% use or depletion.
    --
    Craige Brooks
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com