how do i chromeplate alumminum ? can it be chromed ? is it dangerous to have this done?
Announcement
Collapse
No announcement yet.
chrome
Collapse
X
-
You need to treat it with Zincate, then nickel, copper and chrome plate it.
See http://www.caswellplating.com/zincate.htm and http://www.caswellplating.com/triple.htm--