I am trying to help a friend plate some gold on pewter. He is using nickle as the primary coat and having a time getting a bright nickle. Does gold have to be put on nickle or would copper work also? Thanks
Announcement
Collapse
No announcement yet.
Gold on pewter
Collapse
X
-
Re: Gold on pewter
You need to Flash Copper, Nickel, then Gold plate.--