  • Rinsing Of Parts

    When using the Triple Plating System, does the piece have to be rinsed after each step (ie;nickel,copper,chrome) with distilled water or will fresh water (hot or cold) suffice, also does this apply when using the SP Degreaser and various pickles

  • #2
    Use distilled water for everything to avoid introducing any impurities into your solutions.
    --
    Mike Caswell
    Caswell Inc