    Can you copy chrome motorcycle exhaust pipes?Will it stand up to the heat?Will it blue faster than reg. triple plate?Thanks for the answers in advance

  • #2
    Sorry, we don't have any information on this, mainly because the bluing that occurs on chrome is somewhat of a mystery itself. It usually only occurs on low quality chrome jobs.

    If you want to experiment, get a Copy Chrome Plug N Plate Kit, plate a small steel item and heat it up to see if it blue's.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com