    It would be to be REALLY thick to fuse...I don't think I stressed this enough in the original post.

    You won't have a problem with fusing.

    Leave a comment:


  • cshu
    started a topic electroless and articulating parts

    electroless and articulating parts

    I noticed a post about electroplating movable parts; the parts may fuse if the plating gets thick. Is that true for electroless plating also? What would be your guess for tank time on a small movable part?