Stop up the ends with putty. This will prevent it plating the inside.
Electroless is best for plating inside tubes, so really isn't want you want here.
Announcement
Collapse
No announcement yet.
Brushed Nickel (elect/non-elect) on a Pistol
Collapse
X
-
Brushed Nickel (elect/non-elect) on a Pistol
Ok I have a Magnum research desert eagle, which I want to do some custom work on, but the problem i have is the bore and the chamber, How would you keep the plating from well plating the inside?
I read the masking areas post. and don think it's apporiate, but ??
Ok and the next question Electro or Non-Electro, whats the difference.
Thank You,