    Sure.

    What metal are you plating and what is the base metal? Are you committed to brush plating, or would immersion plating be ok too?

    Leave a comment:


  • Dean
    started a topic Plating process.

    Plating process.

    I used a plating process in the past that was called \"Selectron Brush Plating\", and from looking at the plating kits, it seems to be that the process is quite similar (it would have to be). I have some ideas for use of the nickel and chrome plating process that would have fit well with the \"Selectron Brush Plating\" process, but I guess they are no longer in the business. Ergo, I come to you, to see if it would be practical to attempt using your processes, to plate the surface area of 20 to 40 square inches, to a depth of less than 1,000th of an inch.