    Can the Nickel plug 'n' plate be used to brighten up existing nickel plate. I have some ornate trim that is 60 yrs old and is in need of help, nickel is missing in places and over all rather dull. What would be the procedure here?

    Thanks,
    Laird

  • #2
    plug n plate

    If you want to nickel plate over existing nickel plate, you need to activate it. Read the section on preparing your solutions in the manual for a nickel activator pickle.


    use dish soap and hotwater to degrease