i just sprayed an object with conductive paint. i then tested it with a volt meter and it didn't show any conductivity. before i plate the object i was wondering if anyone has had success with this paint?
Announcement
Collapse
No announcement yet.
conductive paint
Collapse
X
-
I assume you're using the Copper based paint?
The part will not register as conductive with a volt meter after painting. It should plate fine though, if you follow the instructions in the manual.--
Mike Caswell
Caswell Inc
http://www.caswellplating.com