    Re: Zinc Brightener

    How much did you add?

    You can plate a larger piece of scrap metal for an hour - that should remove the brighteners and allow you to plate the dull/cad look.

    Leave a comment:


  • 68goat
    started a topic Zinc Brightener

    Zinc Brightener

    How long does the brightener remain active in a 4 gallon batch of copy zinc. I plated a couple of pieces and would now like to plate a couple of pieces with copy cad.

    Thanks