Re: Anode positioning
The more anodes the better.
Having anodes on each side will help make for a more even plate.
Leave a comment:
-
Anode positioning
In a 4 gallon batch of copy zinc, would it be reccomended running two 4x8 anodes for larger flat pieces (one on each side of bucket) or is one anode enough.
ThanksTags: None