Yes, you'll need to polish them first. You'll also need some Zincate solution so that the plate will stick on the aluminum.
Announcement
Collapse
No announcement yet.
sandblasting
Collapse
X
-
sandblasting
Hi Iam interested on the copy chrome kit or the electroless krome kit. The parts that I want to plate are all aluminum but I think I have made a mistake on preparing them.
I sandblasted them which left the surface of the parts very pourus and rough.
Do I have to polish them in order to plate the part and get the mirror like surface?
Thanks.Tags: None