  • mcaswell
    replied
    Depends what you want to plate onto it. Gold, silver, brass, copper, chrome will go directly onto it.

    More Copy Chrome or Nickel requires activation with Pickle #3.

    Leave a comment:


  • SUPRARACER
    started a topic Replate copy chrome

    Replate copy chrome

    Can you plate onto copy chrome by activating it with pickel #3 or do you have to deplate and then replate.

    Thanks
    John