    My Caswell silver solution lately is producing a very golden color insted of a nice silvery white. I have always user a sterling silver fork as the anode and plate at 3 votes. The solution is less then a year old and not used much. What gives?? Gus c.
    I'm into modifying and inventing

  • #2
    Sterling silver is only approx 92% pure silver. You'll have better success using a pure silver anode.
    --
    Mike Caswell