My Nickle Anodes are pitting up. they got little holes in them bad. it did'nt do it befor. could you tell me what mite be doing wrong or is that the way it works. i clean them every time i use them. I only used them 8 times. and the last time i used them i dont know if they worked my power went off befor i got to do any plating and i have not plated anything else yet.
Announcement
Collapse
No announcement yet.
Anodes pitting
Collapse
X
-
Without more details, all I can say is that this is probably due to the normal operating of the plating system. The anodes are going to look pretty beat up as they are used up. If you can't plate anything with them any more, there may be another issue. Post a problem in our support section.--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
-
About 20 square feet.--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Comment
Comment