Hello,
What steps are required to use copy chrome on a aluminum part? I would like to dip the parts in the copy chrome, so how do i do that with theincluded power supply? Do i just attach both aligator clips and dip it in? Also, when using the zincate before hand, do i just put my part on a wire or something and dip it in there?
Finally, how do i store the zincate after each use and how long does it stay good for?
Thanks
Matt
What steps are required to use copy chrome on a aluminum part? I would like to dip the parts in the copy chrome, so how do i do that with theincluded power supply? Do i just attach both aligator clips and dip it in? Also, when using the zincate before hand, do i just put my part on a wire or something and dip it in there?
Finally, how do i store the zincate after each use and how long does it stay good for?
Thanks
Matt