    replied
    Yes, that's correct.

    Leave a comment:


  • tbloss001
    replied
    Okay, now I don't mean to sound dense, but does that mean I do need to use two things to strip the nickle and the chrome?

    First pickle #2 for the chrome THEN pickle #3 for the nickle?

    Leave a comment:


  • mcaswell
    replied
    Use pickle #2 to deplate chrome. Page 47 of the newest manual.

    Leave a comment:


  • tbloss001
    started a topic Can you electro strip chrome with pickle #3?

    Can you electro strip chrome with pickle #3?

    Can you electro strip chrome with pickle #3?
    I know you can de-plate nickel with pickle #3, but the manual doesn't say anything about stripping chrome.

    Do I have to use one solution to strip the chrome, and then use the pickle to strip the nickle?

    Thanks for any info.