    I have a small, decorative pen holder that is SOLID BRASS with a gold finish on it. I want to Chrome Plug 'N Plate it because I need it to be a shiny chrome color. Do I have to remove the gold finish or can I just plate over it? If I have to remove the gold finish, what is the best way? Thanks for your time.

  • #2
    If it's gold plated, you can plate directly over it. If it's a painted (or other)finish, you'll need to strip it.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com

    Comment


    • #3
      Thanks so much for your help. The item is gold plated and I'm happy to know now that I can just plate right over it. Thanks again.