Just wondering if a 15v 20A is sufficient for plating copycrome and nickel. Or should I buy a 15v 30A. Any suggestions. What do most of you use?
Announcement
Collapse
No announcement yet.
Is a 15v 20A good for most plating jobs with copycrome and nickel
Collapse
X
-
Re: Is a 15v 20A good for most plating jobs with copycrome and nickel
Nickel & CC require 0.07 amps per square inch. 30 amps will plate parts up to approx 420 sq in.--
Lance Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Please support the moderators on our site by leaving reputation for their helpful posts. Read more here.
Comment