  • copy chrome problems

    i am using the 1.5 gal kit and i am trying to plate some aluminum door handles. i can't get it to plate even and the plating peels off some parts of the handle. i can do a bolt fine. the plating will cover some parts of the handles a grey color and when i try to buff it out the plating will come off.

  • #2
    Re: copy chrome problems

    If the plate is peeling this is a prep problem
    what steps are you taking in your prep of the parts you are plating
    Jim Eaton

    Comment