    Can anyone out there tell me the best placement of anodes in the wheel kit tanks to be able to plate to the total depth of the tanks, or should I just strip the anodes by length and go as deep as I can and use extra anodes?

  • #2
    Re: simple question

    On page 11 of the manual there is a clear description on how to cut a strip on the anode for hanging I use this method to center the anode in the solution. My tanks will only holds a 16" wheel I keep my anode aprox 5" away form the part with a surface are this large
    hope this helps
    Jim Eaton