Announcement

Collapse
No announcement yet.

Rust on Copy Chrome?

Collapse
X
 
  • Filter
  • Time
  • Show
Clear All
new posts

  • Rust on Copy Chrome?

    I'm using the immersion method with the plug n plate kit and the parts seem to be plated when I am finished, but after some time, a month or so, the parts seem to have large rust spots on them. See the pictures. I cannot feel any difference in level when I scrape a knife across the rusted area and the plated area, so it seems that there is rust coming through the plate?? I am polishing, then de-greasing with a carb cleaner and directly into the immersion for about 5 minutes or so with a current of 40ma per sq inch. What is this about?

    Thanks,
    Dave
    Attached Files

  • #2
    Re: Rust on Copy Chrome?

    Honestly Dave this simply sounds like you did not get a heavy enough coat on the piece
    Jim Eaton