    Hello,

    I have another noob question. How would I get the chrome to be different colors like in the picture I have included with this thread? If someone could point me in the correct direction I would greatly appreciate it!
    Attached Files

  • #2
    Re: Colored Chrome Question

    Ummm anyone? Bueller..........Bueller...........Bueller........ .
    No one has any ideas?

    Comment


    • #3
      Re: Colored Chrome Question

      WIKD,

      Try this link. It is a spray on Chrome system that looks incredible.

      http://www.sprayonchrome.com/index2.html

      This may be what you are looking for.
      Curtis Ashcroft
      M and C's Plating & Powder Services

      Comment


      • #4
        Re: Colored Chrome Question

        Thanks Ash,

        Alas I would hate to have to dump more money after acquiring the Acid Copper / Copy Chrome, power supply, airbrush, ect....