    I have used the electroless nickle and gold tank kits with great results. I got the 3.5 copy chrome kit with a 5 amp power supply.I live in the dessert and even with air conditioning the temp is between 80-90 degress. With about .7-1 amp and following the book I still get brown or black smudges on the surfaces. What is the maximun temp to use with the cc? thank you
    overlandindustries

  • #2
    Re: brown cc

    Originally posted by crob241 View Post
    I have used the electroless nickle and gold tank kits with great results. I got the 3.5 copy chrome kit with a 5 amp power supply.I live in the dessert and even with air conditioning the temp is between 80-90 degress. With about .7-1 amp and following the book I still get brown or black smudges on the surfaces. What is the maximun temp to use with the cc? thank you
    The Max temp i have used is 110 degress
    Jim Eaton

    Comment


    • #3
      Re: brown cc

      Will the brown buff off? I rinse part well after copy chrome and blow dry with air. Then wax.