    Alright... i do have some background and experience working with carbs. Primarily holley carb body/dichromate. The weber carb body however doesn't come in that gold finish... and the material does machine a bit differently. It looks like the copy cad/zinc kit would suffice... however, in my past experience we had never used power supply/anode/cathode... believe it was electroless.... comments, suggestions... am i going crazy in my old age

    will the black chromate work as well (as the yellow/gold) on these cast carb bodies?

    Thanks,

    Matt

  • #2
    Re: Weber DCOE carb plating suggestion....

    I think as long as you prep the part the Black Chrome will work and look great
    Jim Eaton

    Comment


    • #3
      Re: Weber DCOE carb plating suggestion....

      Could the look you are looking for be gold Alodine? That doesn't use electricity. It's used on some airplane engine parts. That sounds like what you described.
      Steve Dold
      http://stevedold.com

      Comment


      • #4
        Re: Weber DCOE carb plating suggestion....

        Originally posted by sdold
        Could the look you are looking for be gold Alodine? That doesn't use electricity. It's used on some airplane engine parts. That sounds like what you described.
        we did use alodine, but only for the baseplates for some reason, i cant recall... different metal obviously.

        definatly used dichromate after an acid etch..... and it definatly wasn't connected to an electrode..... oh well, wish i would have realized then that i might want to understand what was going on.