Follow up to a previous post concerning using plug n plate on existing nickel. The reply was to pickle first. Info I omitted was that this is on pot metal, does this alter the procedure??
Thank you,
Laird
Thank you,
Laird
Welcome To The Caswell Inc Forums - The Place To Be For Metal Finishing Enthusiasts!
We notice that you are not currently registered on our site, or are not logged in. Registration is FREE and allows you to post questions on our forums, post pictures, access Technical Support, place orders for products and much, much more! Why not take a moment and register? Just click the Register Link above.