Polishing bead blasted aluminum

Collapse
X
 
  • Filter
  • Time
  • Show
Clear All
new posts

  • mtlplshr
    replied
    Re: Polishing bead blasted aluminum

    the cast alum. i've done required some prity heavy sanding to get all the tiny pits out.you can get it shiney with emery but you will have black pits on the surface.the sanding really makes the difference and i think is well worth the effort.

    Leave a comment:


  • MDill
    started a topic Polishing bead blasted aluminum

    Polishing bead blasted aluminum

    I've got some cast aluminum parts that have been beadblasted (fine glass bead). If I want to polish them will a black compound/sisal combo be enough to smooth things out or should I expect to do some sanding or other heavy removal (greaseless compound).

    Matt