hello all,i attempted something alittle different just for fits and giggles.
instead of thinner or a-tone i used never dull between compounds.it looks kinda like house insulation and is treated,gets into tight spots and wipes off
easy.i don't suggest using it during the final stages of polishing but does come in handy for quick spot clean up and shine.
instead of thinner or a-tone i used never dull between compounds.it looks kinda like house insulation and is treated,gets into tight spots and wipes off
easy.i don't suggest using it during the final stages of polishing but does come in handy for quick spot clean up and shine.