    What type of casting are the bores in? Gun barrels? Pipes? This could be as simple as getting a cartridge sanding roll kit along with a few felt bullet and/or mushroom bobs. (If you can find them that small.)

    Leave a comment:


  • edwin247
    replied
    Is anyone doing this?

    Leave a comment:


  • edwin247
    started a topic SS and Aluminum small ID bore polishing

    SS and Aluminum small ID bore polishing

    I need to polish small bores in both 1/4" and 3/8" ID does anyone have some hits/links to polishing items for these small bores? What would you use for a wheel or bobbin.