    Does anybody have any suggestions to remove the rust and oxidation stains from this steam engine bell? It is 100% better that when we started by just using various buffing wheels and black rouge.

    Whippany Railway Museum, NJ

  • #2
    Re: Steam Engine Bell

    the best thing ive found for removing rust is oxalic acid
    "A stupid man's report of what a clever man says is never accurate because he unconsciously translates what he hears into something he can understand.
    Custom Anodising

    Comment


    • #3
      Re: Steam Engine Bell

      Depending on the metal you might like to read this
      ----------