Hello,
I have a magnesium front sprocket cover from a motorocycle that I have begun polishing.
I have it all stripped of paint and have begun polishing it.
On a small test area it started polishing really well with the black emery, brown tripoli and red rouge that I have. The problem is with the final compound.
Since magnesium is so soft the white diamond compound still leaves noticable scratches, even with a loose cotton wheel!
Is there a better compound to use for magnesium or should I try some different method?
Thanks,
etyrrany
I have a magnesium front sprocket cover from a motorocycle that I have begun polishing.
I have it all stripped of paint and have begun polishing it.
On a small test area it started polishing really well with the black emery, brown tripoli and red rouge that I have. The problem is with the final compound.
Since magnesium is so soft the white diamond compound still leaves noticable scratches, even with a loose cotton wheel!
Is there a better compound to use for magnesium or should I try some different method?
Thanks,
etyrrany