i have a loose cotton wheel that i used red rouge on two times. just wanted to experiment with the red and see what it did, etc. wheel was new, unused.
(i thought red didn't 'scratch' but this one does!- lol) anyway....i let it soak in a bucket of hot soapy water for 10-15 mins. figured that would let the waxy stuff kinda melt and get loose, etc.
shook it around in the water for a minute or two, and rinsed out thoroughly under hot tap water.
think its ok to use with my white now?
(i thought red didn't 'scratch' but this one does!- lol) anyway....i let it soak in a bucket of hot soapy water for 10-15 mins. figured that would let the waxy stuff kinda melt and get loose, etc.
shook it around in the water for a minute or two, and rinsed out thoroughly under hot tap water.
think its ok to use with my white now?
Comment