the wheel i'm currently using for the first 'stage' isn't perfectly round!! hahaha-- of all the blasted things. i noticed when i raked it today....some of the surface wasnt disturbed very much.
luckily had a new one- different manf'r--- and bingo... smooth sailing. thank goodness!!! ive been getting really frustrated.
boy....won't forget this little 'lesson'
luckily had a new one- different manf'r--- and bingo... smooth sailing. thank goodness!!! ive been getting really frustrated.
boy....won't forget this little 'lesson'