I have an old british bike with chrome fenders. The chrome has small specks of rust on the surface. Is it possible to polish the chrome and remove these specks or is a re-chrome necessary?
Announcement
Collapse
No announcement yet.
Chrome polishing
Collapse
X
-
Re: Chrome polishing
Depending on how deep the rust goes, it may be possible to just polish it out. It certainly wouldn't be a waste of time or money to try.
Polish chrome using a white buffing compound and a cotton wheel.--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
-
Re: Chrome polishing
would that be a loose cotton wheel or a spiral sewn wheel? Those are made of cotton to right?
Comment
-
Re: Chrome polishing
Either one would do. A spiral wheel will do the work faster. A loose wheel will give a lighter touch.--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Comment
-
Re: Chrome polishing
The spiral sown would go faster... But would the loose cotton provide a better finish? Maybe this person should do a two stage polishwhat ya think CASWELL?