Be sure to get a sisal wheel for the first buffing, spiral won't be enough to cut it even with the emery. I've had very good results on carbon steel with sisal/emery, spiral/emery, loose cotton/white, loose cotton/rouge. I dropped the spiral/tripoli as the third buff when I didn't notice any difference in the finish. I spent twice as much time on the white and it helped tremendously with the finer scratches. They do have the green compound specifically made for stainless but I am very pleased with my results so really haven't had a need to try it yet.
-
Read the Polishing instructions here. Lots of useful info in there. I don't think you'll find you'll need ONE compound, but probably several to get the desired shine.
Good luck
Leave a comment:
-
Polishing Stainless Steel
Can someone recommend a compound and buffing wheel to polish stainless steel without showing the buffing circles?Tags: None